WANG Rongguang

Profile Research field Research achievement

 

Books
No.Title URL, Autour Type, Publisher, Publication date, Range, ISBN 
1
Microscopy Series Vol.1 --Science, Technology and Education of Microscopy: an Overview , , , Mar. 2003, ,  

 

Academic papers
No.Title URL, Journal, Vol( No), Start Page- End Page, Publication date, DOI 
1
Influence of Dissolved Oxygen on DL-EPR Behavior of SUS329J4L Duplex Stainless Steel after Convection Cooling , Journal of the Society of Materials Science, Japan, 70( 1), 49- 56, Jan. 2021,  
2
Determination of Cooling Intensity Using Transient Heat Transfer Technique at Gas Quenching in Vacuum Heat Treating Furnace , Journal of the Society of Materials Science, Japan, 69( 5), 387- 394, May. 2020,  
3
Effect of helium implantation on the hydrogen retention of Cr2O3films formed in an ultra-lowoxygen environment , International Journal of Hydrogen Energy, 44,  26685- 26697, Oct. 2019, https://doi.org/10.1016/j.ijhydene.2019.08.122 
4
Using Atomic Force Microscopy to Measure Thickness of Passive Film on Stainless Steel Immersed in Aqueous Solution , Scientific Reports, 9,  13094-1- 13094-11, Sep. 2019, https://doi.org/10.1038/s41598-019-49747-0 
5
Synthesis, characterization, and transport properties of Nafion-polypyrrole membrane for direct methanol fuel cell (DMFC) application , Journal of Solid State Electrochemistry, 23( 8), 2423- 2433, Aug. 2019,  
6
Electropolymerization and corrosion resistance of polypyrrole on nickel bipolar plate for PEM fuel cell application , Materials today: proceedings, 22( Part 1), 52- 56, Aug. 2019,  
7
Electrochemically roughened silver surface versus fractal leaf-shaped silver crystals for surface-enhanced Raman scattering investigation of polypyrrole , Journal of Solid State Electrochemistry, 23( 6), 1811- 1827, Jun. 2019, https://doi.org/10.1007/s10008-019-04288-4. 
8
Characteristic and behavior of an electrodeposited chromium (III) oxide/silicon carbide composite coating under hydrogen plasma environment , Fusion Engineering and Design, 143,  137- 146, Jun. 2019,  
9
Suppression effect of ultrasound on pitting corrosion of SUS304 stainless steel in various NaCl solutions , Science China Technological Sciences, 62( 4), 551- 558, Feb. 2019, https://doi.org/10.1007/s11431-018-9383-3 
10
Hydgrogen permeation properties of CrxCy@Cr2O3/Al2O3 composite coating derived from selective oxidation of a Cr-C alloy and atomic layer deposition , International Journal of Hydrogen energy, 45,  21133- 21141, Nov. 2018, https://doi.org/10.1016/j.ijhydene.2019.02.035 
11
Corrosion behaviour of mild steel in chloride solutions with Na2HPO4 additive and the development of antifreeze , Corrosion Engineering, Science and Technology, 53:sup1,  67- 74, Jul. 2018, DOI: 10.1080/1478422X.2017.1370853 
12
Double-loop electrochemical potentiokinetic reactivation behaviour of continuously cooled SUS329J4L duplex stainless steel , Corrosion Engineering, Science and Technology, 53:supp1,  44- 50, Jul. 2018, DOI: 10.1080/1478422X.2017.1372246 
13
Formation of Multiscale Protrusions on Commercially Pure Titanium and Stainless Steel by Two-Stage Sputter-Etching Using Different Cathode Disks , Materials Transaction, 59( 7), 1198- 1205, Jul. 2018, doi:10.2320/matertrans.M2018025 
14
Comparison study between corrosion protection of polypyrrole synthesized on stainless steel from phthalate and saccharinate aqueous medium , Polymer Testing, 67,  302- 308, May. 2018, https://doi.org/10.1016/j.polymertesting.2018.03.022  
15
Constructing superhydrophobic WO3@TiO2 nanoflake surface beyond amorphous alloy against electrochemical corrosion on iron steel , Applied Surface Science, 436,  527- 535, Apr. 2018, 10.1016/j.apsusc.2017.11.211 
16
Electro-wetting behavior of sodium chloride aqueous solution on hydrophobic surfaces of stainless steel and its influence on polarization , Materials Transaction, 58( 12), 1670- 1678, Dec. 2017, 10.2320/matertrans.M2017224 
17
In situ surface-enhanced Raman scattering investigation of poly (5-amino-1,4-naphthoquinone) using roughened electrodes and metal colloids , Synthetic Metals, 231,  80- 88, Sep. 2017, 10.1016/j.synthmet.2017.06.019 
18
Formation of Fine Protrusions by Sputter Etching of Commercially Pure Titanium , Tetsu-to-Hagane, 81( 4), 211- 220, Apr. 2017, 10.2320/jinstmet.J2016064 
19
Influence of Humidity on Friction Forces in Point-Contact under Small Loads , Materials Transaction, 58( 2), 236- 242, Feb. 2017, 10.2320/matertrans.M2016371 
20
Effect of Crystal Plane Orientation on Protrusion Formation during Sputter-Etching of SUS410 Stainless Steel , Tetsu-to-Hagane, 103( 2), 101- 110, Feb. 2017,  
21
SECM investigation of electrochemically synthesized polypyrrole from aqueous medium , J Appl Electrochem, 46( 12), 1199- 1209, Dec. 2016, 10.1007/s10800-016-1002-9 
22
Effect of electrolytic conditions on PANi electrosynthesis on stainless steel: A new application to polycarboxy-benzoic acids removal from industrial effluents , Progress in Organic Coatings, 101,  233- 239, Dec. 2016, 10.1016/j.porgcoat.2016.06.021 
23
Effect of plasma nitriding on the compressive strength of multi-functional fine protrusions formed by sputter-etching of stainless steels , Transactions of the JSME, 82( 838), 16-00059-1- 16-00059-15, Jun. 2016, 10.1299/transjsme.16-00059 
24
Effect of ultrasound on initiation, growth and repassivation behaviours of pitting corrosion of SUS304 steel in NaCl aqueous solution , Corrosion Engineering Science and Technology, 51( 3), 201- 210, May. 2016, 10.1179/1743278215Y.0000000046 
25
Electrochemical and spectroscopical studies of polypyrrole synthesized on carbon steel from aqueous medium , Synthetic Metals, 209,  11- 18, Nov. 2015, 10.1016/j.synthmet.2015.06.017 
26
Effect of plasma nitriding on the strength of fine protrusions formed by sputter etching of AISI type 420 stainless steel, , Surface Coating & Technology, 272,  298- 308, Jun. 2015, 10.1016/j.surfcoat.2015.03.048 
27
Enhancement of Visible Light Absorbance and Hydrophobicity by Sputter-Coating of PTFE onto Fine Protrusions Formed by Sputter-Etching of Steels , Materials Transactions, 56( 1), 91- 98, Jan. 2015, 10.2320/matertrans.M2014270 
28
Formation of Fine Protrusions by Sputter Etching of Martensitic Stainless Steels , Tetsu-to-Hagane, 100( 5), 647- 655, May. 2014, 10.2355/tetsutohagane.100.647 
29
Corrosion behaviour of SUS304 stainless steel after UV-O3 treatment in sealed air environment, , Surface Engineering, 27( 3), 174- 179, Nov. 2013, 10.1179/026708409X12543892706575 
30
Hydrophobicity and corrosion resistance of steels coated with PFDS film , Surface Engineering, 29( 4), 255- 263, Sep. 2013, 10.1179/1743294412Y.0000000101 
31
A Simple Method for Acrylonitrile Butadiene Styrene Metallization , Surface & Coatings Technology, 224,  71- 76, Jun. 2013, 10.1016/j.surfcoat.2013.02.050 
32
Formation of fine protrusions on steel sheets and wires by sputter etching , Tetsu-to-Hagane, 98( 12), 658- 666, Dec. 2012, 10.2355/tetsutohagane.98.658 
33
Superhydrophobicity produced by vapor deposition of hydrophobic layer onto fine protrusions formed by sputter-etching of steels , Surface & Coatings Technology, 210,  113- 121, Oct. 2012, 10.1016/j.surfcoat.2012.09.001 
34
Coating Damage Fracture of WC Therrnal Spray Coatings by Corrosion Fatigue , Journal of Thermal Spray Technology, 48( 4), 149- 155, Oct. 2011, 10.11330/jtss.48.149 
35
Growth behavior of pitting corrosion of SUS304 stainless steel in NaCl aqueous solution when applying ultrasound with different frequencies , Zairyo-to-Kankyo / Corrosion Engineering of Japan, 60( 2), 66- 68, Feb. 2011, 10.3323/jcorr.60.66 
36
@U Growth behavior of pitting corrosion of SUS304 stainless steel in NaCl aqueous solution when applying ultrasound with different frequencies , Corrosion Engineering, 60( 2), 47- 49, Feb. 2011,  
37
Galvanic corrosion behavior between aluminum and copper caused by NaCl aqueous solutions , Zairyo-to-Kankyo / Corrosion Engineering of Japan, 60( 1), 22- 27, Jan. 2011, 10.3323/jcorr.60.22 
38
Wettability of Sodium Chloride Aqueous Solutions on SUS304 Stainless Steel with Current Flow , Materials Transactions, 51( 2), 359- 365, Feb. 2010, 10.2320/matertrans.M2009336 
39
Corrosion and Wear Resistances of Ni-P-Al2O3 Composite Film Prepared by Electroless Plating , Materials Science Forum, 654-656,  2767- 2770, Jan. 2010, 10.4028/www.scientific.net/MSF.654-656.2767 
40
Nano-Indentation Characteristics of Surface Layer with Fine Conical Protrusions Formed by Sputter Etching of W-Cr Tool Steel , , 73( 11), 870- 877, Nov. 2009, 10.2320/jinstmet.73.870 
41
Deformation and Delamination Behavior of Sputter-deposited Film on the Conical Protrusions Formed by Sputter-etching of Stainless Steel Wire , Surface & Coatings Technology, 204( 9), 108- 114, Sep. 2009, 10.1016/j.surfcoat.2009.06.046 
42
Influence of input power to vibrator and vibrator-to-specimen distance of ultrasound on pitting corrosion of SUS304 stainless steel in 3.5% chloride sodium aqueous solution , Corrosion Science, 51( 8), 1604- 1610, Aug. 2009, 10.1016/j.corsci.2009.04.008 
43
Adhesion of Atmospheric Micro-contaminants on SUS304 Steel Surface and Removal by UV Illuminataion , Materials Transaction, 50( 7), 1798- 1804, Jul. 2009, 10.2320/matertrans.M2009026 
44
Adhesion of Atmospheric Micro-contaminants on SUS304 Steel Surface and Their Removal by UV-O3 Treatment , Journal of the Japan Institute of Metals, 72( 11), 856- 862, Nov. 2008, 10.2320/jinstmet.72.856 
45
Observation of Micro-contaminants on Pure Chromium Surface by AFM and Removing Them by UV Light , Surface and Interface Analysis, 40( 9), 1284- 1288, May. 2008, 10.1002/sia.2879 
46
Formation of Conical Protrusions on SUS304 Stainless Steel by Sputter Etching and the Corrosion Behavior of Surface , Journal of the Japan Institute of Metals, 72( 2), 117- 124, Feb. 2008, 10.2320/jinstmet.72.117 
47
nfluence of ultrasound on pitting corrosion and crevice corrosion of SUS304 stainless steel in chloride sodium aqueous solution , Corrosion Science, 50( 2), 325- 328, Feb. 2008, 10.1016/j.corsci.2007.11.001 
48
Improvement of Corrosion Fatigue Strength of WC Coated Steel by Adjusting Powder Composition and Spraying Pressure , Research Bulletin of the Hiroshima Institute of Tech, 42,  7- 14, Feb. 2008,  
49
Influence of additives and hot-press sintering on lipophilic properties of silicon nitride ceramics , Materials Science Forum, 539-543,  2687- 2692, Jun. 2007,  
50
すき間を有するSUS304ステンレス鋼の腐食挙Influence of Application of Ultrasonic Wave on Corrosion Behavior of SUS304 Stainless Steel With Crevice , Journal of the Japan Institute of Metals, 71( 6), 511- 516, Jun. 2007, 10.2320/jinstmet.71.511 
51
Corrosion Behavior of Pure Iron by Different Droplet Volume of Sulfuric Acid Solution, , Materials Transaction,, 48( 6), 1451- 1457, Jun. 2007, 10.2320/matertrans.MRA2006354 
52
Effect of Ultrasonic Wave on the Growth of Corrosion Pits on SUS304 Stainless Steel, , Materials Transactions, 48( 5), 1017- 1022, May. 2007, 10.2320/matertrans.48.1017 
53
Surface strain measurement of thermally sprayed ceramics coatings under static and cyclic loadings and its application to detection of delamination, , Materials Transactions, 48( 4), 769- 774, Apr. 2007, 10.2320/matertrans.48.769 
54
Influence of SiO2 addition on Mechanical and Lipophilic properties of silicon nitride ceramics , Journal of the Japan Institute of Metals, 71,  128- 134, Jan. 2007, 10.2320/jinstmet.71.128 
55
Fundamental analysis of pure titanium and its alloy corrosion and water wettability in solution , Journal of the Japan Institute of Metals, 70( 12), 962- 967, Dec. 2006, 10.2320/jinstmet.70.962 
56
Water wettability of commercial pure titanium and an alloy altered by immersion in aqueous NaF solution , Journal of the Japan Institute of Metals, 70( 12), 956- 961, Dec. 2006, 10.2320/jinstmet.70.956 
57
Influence of droplet volume of sulfuric acid solution on corrosion behavior of pure iron , Journal of the Japan Institute of Metals, 70( 11), 929- 935, Nov. 2006, 10.2320/jinstmet.70.929 
58
Corrosion behavior of pure iron beneath a micro-droplet of sulfuric acid solution investigated by atomic force microscopy , Scripta MATERIALIA, 55,  633- 636, Oct. 2006, 10.1016/j.scriptamat.2006.06.011 
59
Formation of Fine and Dense Conical Carbides on Tool Steel Surface by Sputter Etching, Materials Transactions , Materials Transactions, 47( 7), 1798- 1804, Jul. 2006, 10.2320/matertrans.47.1798 
60
Surface strain and delamination generation of thermally sprayed ceramics coating under static and cyclic load , Journal of Japan Thermal Spraying Society, 43( 3), 73- 78, Jul. 2006,  
61
Producing a micro-droplet of dilute sulphuric acid on a pure iron surface and observing its corrosion behaviour by means of atomic force microscopy , Transactions of Nonferrous Metals Society of China, 16,  s749- s752, Jun. 2006, 10.1016/S1003-6326(06)60294-X 
62
Residual stress measurement and evaluation on ceramics with X-ray and indentation method , Key Engineering Materials, 321-323,  1348- 1352, Jun. 2006,  
63
Analysis of air adsorptive on solid surfaces by AFM and XPS , Transactions of Nonferrous Metals Society of China, 16,  s753- s758, Jun. 2006,  
64
Effect of the application of an ultrasonic wave on the growth of corrosion pits on SUS304 stainless stee , , 70( 3), 226- 232, Mar. 2006, 10.2320/jinstmet.70.226 
65
Influence of ultraviolet light irradiation on corrosion behavior of weathering steel with and without TiO2-coating in 3 mass% NaCl solution , Scripta MATERIALIA,, 53,  1303- 1308, Dec. 2005, 10.1016/j.scriptamat.2005.07.039 
66
Influence of Additives and Hot-Press Sintering on Mechanical and Lipophilic Properties of Silicon Nitride Ceramics , Materials Transactions, 46( 9), 2041- 2046, Sep. 2005, 10.2320/matertrans.46.2041 
67
Influence of Attractive Force on Imaging Micro-Droplets of Water by Atomic Force Microscope , Surface and Interface Analysis, 37,  1105- 1110, Sep. 2005, 10.1002/sia.2085 
68
Formation of Conical Carbides on the Surface of Stainless and Alloy Steels by Sputter-Etching , Journal of the Japan Institute of Metals, 69( 3), 312- 219, Mar. 2005, 10.2320/jinstmet.69.312 
69
Observation by Atomic Force Microscope of Corrosion Product during Pitting Corrosion on SUS304 Stainless Steel , Scripta MATERIALIA, 52,  227- 230, Feb. 2005, 10.1016/j.scriptamat.2004.09.024 
70
An AFM and XPS study of corrosion caused by micro-liquid of dilute sulfuric acid on stainless steel , Applied Surface Science, 227,  399- 409, Apr. 2004, 10.1016/j.apsusc.2003.12.019 
71
XPS Analysis and Atomic Force Microscopy Observation of Micro-liquids adsorbed on Pure Iron and Copper Surfaces , Materials Forum Science, 449-452,  1025- 1028, Jan. 2004,  
72
Observation of Micro- Water droplets on Several Materials Surfaces and Evaluation of Wettability by Means of AFM , Transactions of the Japan Society of Mechanical Engineers, 67( 8), 404- 409, Aug. 2003, 10.1299/kikaia.69.1657 
73
Evaporation and Condensation Behaviors of Micro- Water Droplets on SUS304 Steel Using AFM , Materials Letters, 57,  16- 17, May. 2003, 10.1016/S0167-577X(02)01235-1 
74
Estimated and Evaluated Residual Stress by Vickers Indentation in Several Structural Ceramics , Journal of the Society of Materials Science, Japan, 52( 1), 82- 88, Jan. 2003, 10.2472/jsms.52.82 
75
High Temperature Fatigue Deformation Measurement of Ceramics Thermally Sprayed SUS304 Steel Using an ESPI System , Materials Science Research International, 9( 1), 69- 74, Jan. 2003,  
76
Nondestructive measurement of fatigue deformation of thermally sprayed steel using ESPI method under high temperature , Journal of Nondestructive Evaluation, 21( 4), 117- 126, Dec. 2002, 10.1023/A:1023837901584 
77
High Temperature Fatigue Deformation Behavior of Ceramics Thermally Sprayed SUS304 Steel Measured with an ESPI System , Journal of the Society of Materials Science, Japan, 51( 12), 1417- 1422, Dec. 2002, 10.2472/jsms.51.1417 
78
Corrosion Behavior of Thermally Sprayed WC Coating in Na2SO4 Aqueous Solution , Materials Transactions, 43( 11), 2860- 2865, Nov. 2002, 10.2320/matertrans.43.2860 
79
Evaluation of the Wettability of Metal Surfaces by Micro- Pure Water Evaluated by Means of Atomic Force Microscopy , Applied Surface and Science, 191( 1/4), 74- 84, May. 2002, 10.1016/S0169-4332(02)00147-2 
80
Micro Pure Water Wettability Evaluation with an AC No Contact Mode of Atomic Force Microscope , Materials Letters, 54( 2/3), 140- 144, May. 2002, 10.1016/S0167-577X(01)00552-3 
81
Micro Pure Water Wettability Evaluation of SUS304 Steel with a Tapping Mode of Atomic Force Microscope , Scripta MATERIALIA, 46,  83- 87, Jan. 2002, 10.1016/S1359-6462(01)01202-7 
82
Study on SCC Behavior of Austenitic Stainless Steels in H2S Saturated Aqueous Solutions Containing Cl- , Journal of Chinese Society for Corrosion and Protection, 19,  47- 53, Feb. 2000,  
83
Effect of N2+ Ion Implantation on the Corrosion Behavior of Pure Titanium , Journal of the Society of Materials Science, Japan, 48( 5), 483- 488, May. 1999, 10.2472/jsms.48.483 
84
ND steel and Its Applying , Pressure Vessel Technology, 15,  36- 39, Jun. 1998,  
85
Selective Corrosion During Stress Corrosion Cracking of 00Cr18Ni5Mo3Si Duplex Stainless Steel , Journal of Chinese Society for Corrosion and Protection, 18,  47- 51, Mar. 1998,  
86
Dew Point Corrosion Properties of ND Steel and Its Application , Corrosion & Protection, 42( 2), 19- 37, Feb. 1997,  
87
Applicability of ND Steel for Resistance to Sulfur Dewpoint Corrosion , Corrosion & Protection, Vol.18( 2), 72- 74, Sep. 1996,  
88
Microstructure and Corrosion Behaviour of Dissimilar-Metal Welded Joints , The Chinese Journal of Nonferrous Metals, Vol.5( Suppl.2), 140- 143, Sep. 1995,  

 

Conference Activities & Talks
No.Title, URL, Presentation date, Vol( No), Start Page- End Page, Publication date 
1
Influence of heat treatment on corrosion and were resistances of mild steel with Ni-P-Al2O3 composite film, , Aug. 2013, ,  1409- 1416,   
2
Influence of frequency and vibrator-to-specimen distance of ultrasound on growth behaviour of pitting corrosion of SUS304 stainless steel in NaCl aqueous solution, , 2011, ,  091-1- 091-10,   
3
Wetting behavior of micro- water on pure chromium, , 2003, ,  OS05W0022-1- OS05W0022-5,   
4
Fatigue behavior of thermally sprayed materials at high temperature, , 2003, ,  OS11W0021-1- OS11W0021-5,   
5
High Temperature Deformation Behaviors of Thermally Sprayed Material Measured with AN ESPI System, , 2003, ,  341- 348,   
6
Effect of Nitrogen Ion Implantation on the Corrosion and Hydride Formation Behavior of Titanium Specimen Sputter-Coated with TiN, , 2001, ,  168- 173,   
7
Resistance to Sulfur Corrosion of Steel-ND and 08Cr2AlMo, , 2001, ,  119- 122,   
8
ND Steel-High Resistance to Sulfur Dewpoint Corrosion, , 1998, 1,  155- 160,   
9
Effect of N2+ ion implantation on the corrosion behavior of pure titanium, , 1998, ,  533- 539,